{"id":609,"date":"2026-07-22T10:50:33","date_gmt":"2026-07-22T02:50:33","guid":{"rendered":"https:\/\/yscltest.aakkkk.com\/about-us\/technical-custom-support\/how-to-read-particle-size-report\/"},"modified":"2026-07-22T10:50:33","modified_gmt":"2026-07-22T02:50:33","slug":"how-to-read-particle-size-report","status":"publish","type":"page","link":"https:\/\/yscltest.aakkkk.com\/de\/about-us\/technical-custom-support\/how-to-read-particle-size-report\/","title":{"rendered":"Anleitung zum Lesen eines Partikelgr\u00f6\u00dfenberichts f\u00fcr Diamantpulver"},"content":{"rendered":"<style>\n  \/* Cell content stays on one line so short labels like \"Sample A\" \/ numbers\n     never wrap character-by-character. Long descriptive cells opt in via .wrap. *\/\n  table.content-table th,\n  table.content-table td { white-space: nowrap; }\n  table.content-table td.wrap,\n  table.content-table th.wrap { white-space: normal; }\n\n  \/* Horizontal scroll fallback when the table would otherwise squeeze cells. *\/\n  .table-wrap { overflow-x: auto; -webkit-overflow-scrolling: touch; }\n  .table-wrap > table.content-table { min-width: 100%; }\n\n  \/* =====  ZEBRA STRIPING (visible alternating row colors)  ===== *\/\n  table.content-table {\n    border-collapse: collapse;\n    border: 1px solid #E5E7EB;\n    background: #FFFFFF;\n  }\n  table.content-table thead th {\n    background: #1F2937;     \/* dark slate header *\/\n    color: #FFFFFF;\n    font-weight: 700;\n    text-align: left;\n    padding: 12px 16px;\n    border-bottom: 2px solid #111827;\n  }\n  table.content-table tbody td,\n  table.content-table tbody th {\n    padding: 11px 16px;\n    border-bottom: 1px solid #E5E7EB;\n    color: #1F2937;\n  }\n  \/* Visible zebra: even rows in light grey *\/\n  table.content-table tbody tr:nth-child(even) td,\n  table.content-table tbody tr:nth-child(even) th {\n    background: #F3F4F6;\n  }\n  \/* Hover highlight (subtle) *\/\n  table.content-table tbody tr:hover td,\n  table.content-table tbody tr:hover th { background: #FDE68A; }\n\n  \/* Star ratings *\/\n  .stars-filled { color: #F2A900; letter-spacing: 1px; }\n  .stars-empty  { color: #D4D4D8; letter-spacing: 1px; }\n<\/style><section data-block-section class=\"mb-16 lg:mb-32\" data-block=\"intro\"><div class=\"contain grid gap-y-4 lg:grid-cols-6 pb-8 lg:pb-16\"><div class=\"lg:col-span-3\"><h1 class=\"text-balance text-5xl\">So lesen Sie einen Partikelgr\u00f6\u00dfenbericht f\u00fcr Diamantpulver<\/h1><\/div><div class=\"w-full prose lg:mt-1 lg:col-span-2 lg:col-start-5\"><div><p>Die Partikelgr\u00f6\u00dfenverteilung (PSD) ist einer der wichtigsten Qualit\u00e4tsparameter zur Bewertung der Schleifleistung von Diamanten. Auf dieser Seite wird die Bedeutung von D10, D50, D90 und D100 erl\u00e4utert und au\u00dferdem wird erl\u00e4utert, wie ein PSD-Bericht durchg\u00e4ngig gelesen wird.<\/p><\/div><\/div><\/div><\/section>\n<figure class=\"not-prose my-12 lg:my-16\"><img width=\"1024\" height=\"819\" src=\"https:\/\/yscltest.aakkkk.com\/wp-content\/uploads\/2026\/07\/Diamond-Powder-Particle-Size-Report-1024x819.webp\" class=\"w-full h-auto rounded-sm\" alt=\"Partikelgr\u00f6\u00dfenbericht f\u00fcr Diamantpulver\" loading=\"lazy\" decoding=\"async\" srcset=\"https:\/\/yscltest.aakkkk.com\/wp-content\/uploads\/2026\/07\/Diamond-Powder-Particle-Size-Report-1024x819.webp 1024w, https:\/\/yscltest.aakkkk.com\/wp-content\/uploads\/2026\/07\/Diamond-Powder-Particle-Size-Report-300x240.webp 300w, https:\/\/yscltest.aakkkk.com\/wp-content\/uploads\/2026\/07\/Diamond-Powder-Particle-Size-Report-768x615.webp 768w, https:\/\/yscltest.aakkkk.com\/wp-content\/uploads\/2026\/07\/Diamond-Powder-Particle-Size-Report-600x480.webp 600w, https:\/\/yscltest.aakkkk.com\/wp-content\/uploads\/2026\/07\/Diamond-Powder-Particle-Size-Report.webp 1402w\" sizes=\"auto, (max-width: 1024px) 100vw, 1024px\" \/><figcaption class=\"text-sm text-textcolor-500 mt-3 text-center\">Auswertung eines Berichts zur Partikelgr\u00f6\u00dfenverteilung (PSD) von Diamantpulver<\/figcaption><\/figure>\n<section data-block-section class=\"mb-16 lg:mb-32 \" data-block=\"cards\"><div class=\"contain\"><h2 class=\"text-xl lg:text-4xl text-balance mb-6\">Was ist die PSD?<\/h2><div class=\"prose max-w-none\"><p>Die Partikelgr\u00f6\u00dfenverteilung (PSD) beschreibt den Partikelgr\u00f6\u00dfenbereich und die prozentuale Verteilung verschiedener Partikelgr\u00f6\u00dfen innerhalb von Diamantpulver.<\/p><p>Da Diamantpulver zerkleinert, geformt, gereinigt und klassifiziert wird, haben die Partikel nicht genau die gleiche Gr\u00f6\u00dfe &mdash; Sie sind innerhalb eines kontrollierten Partikelgr\u00f6\u00dfenbereichs verteilt.<\/p><p><strong>PSD bietet umfassende Informationen \u00fcber:<\/strong><\/p><ul style=\"list-style:none;padding:0\"><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Partikelgr\u00f6\u00dfenbereich<\/li><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Gleichm\u00e4\u00dfige Verteilung<\/li><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Verh\u00e4ltnis von feinen und groben Partikeln<\/li><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Konsistenz von Charge zu Charge<\/li><\/ul><p><strong>PSD wirkt sich direkt auf die Schleifleistung von Diamanten aus:<\/strong><\/p><ul style=\"list-style:none;padding:0\"><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Materialabtragsrate (MRR)<\/li><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Schneidleistung<\/li><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Oberfl\u00e4cheng\u00fcte<\/li><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Prozessstabilit\u00e4t<\/li><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Prozessausbeute<\/li><\/ul><\/div><\/div><\/section><section data-block-section class=\"mb-16 lg:mb-32 \" data-block=\"cards\"><div class=\"contain\"><h2 class=\"text-xl lg:text-4xl text-balance mb-6\">D10 \/ D50 \/ D90 \/ D100<\/h2><div class=\"prose max-w-none\"><p>D-Werte stellen charakteristische Partikeldurchmesser bei bestimmten kumulativen Verteilungsprozents\u00e4tzen dar.<\/p><div class=\"table-wrap\">\n<table class=\"content-table\">\n    <thead><tr><th>Parameter<\/th><th>Definition<\/th><\/tr><\/thead>\n    <tbody>\n        <tr><td>D10<\/td><td>10 % kumulative Partikelgr\u00f6\u00dfe &mdash; Feinpartikelindikator<\/td><\/tr>\n        <tr><td>D50<\/td><td>50 % kumulative Partikelgr\u00f6\u00dfe (mittlere Partikelgr\u00f6\u00dfe)<\/td><\/tr>\n        <tr><td>D90<\/td><td>90 % kumulative Partikelgr\u00f6\u00dfe &mdash; Grobpartikelkontrolle<\/td><\/tr>\n        <tr><td>D100<\/td><td>Maximal erkannte Partikelgr\u00f6\u00dfe<\/td><\/tr>\n    <\/tbody>\n<\/table><\/div><p class=\"mt-6\">Im Allgemeinen gilt: D10 gibt den Feinpartikelgehalt an, D50 ist die prim\u00e4re Arbeitspartikelgr\u00f6\u00dfe, D90 spiegelt die Grobpartikelkontrolle wider und D100 gibt die maximal erkannte Partikelgr\u00f6\u00dfe an.<\/p><p><strong>Beispiel:<\/strong> Wenn D50 = 5 &mu;m ist, sind 50 % der Diamantpartikel kleiner als 5 &mu;m und die \u00fcbrigen 50 % gr\u00f6\u00dfer als 5 &mu;m.<\/p><\/div><\/div><\/section><section data-block-section class=\"mb-16 lg:mb-32 \" data-block=\"cards\"><div class=\"contain\"><h2 class=\"text-xl lg:text-4xl text-balance mb-6\">D10 &mdash; Feinkornkontrolle<\/h2><div class=\"prose max-w-none\"><p>D10 = 1 &mu;m bedeutet, dass etwa 10 % der Partikel kleiner als 1 &mu;m sind. D10 beschreibt vor allem den Ultrafeinpartikelanteil und die Leistungsf\u00e4higkeit der Klassierung.<\/p><p><strong>Ein gut kontrollierter D10-Wert tr\u00e4gt zur Verbesserung bei:<\/strong><\/p><ul style=\"list-style:none;padding:0\"><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Reduzieren Sie Verarbeitungsschwankungen<\/li><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Verbessern Sie die Konsistenz der Oberfl\u00e4chenbearbeitung<\/li><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Verbessern Sie die Stabilit\u00e4t der Pr\u00e4zisionsbearbeitung<\/li><\/ul><p><strong>Typische Anwendungen:<\/strong> optisches Glaspolieren, Halbleiterwaferbearbeitung, Saphir-Pr\u00e4zisionsschleifen, Ultrapr\u00e4zisionspolieren.<\/p><\/div><\/div><\/section><section data-block-section class=\"mb-16 lg:mb-32 \" data-block=\"cards\"><div class=\"contain\"><h2 class=\"text-xl lg:text-4xl text-balance mb-6\">D50 &mdash; Median-Partikelgr\u00f6\u00dfe<\/h2><div class=\"prose max-w-none\"><p>D50 ist in der Regel der wichtigste Referenzparameter bei der Auswahl von Diamantpulver. Es bestimmt die Schleifeffizienz, die Schneidf\u00e4higkeit und die Materialabtragsrate.<\/p><div class=\"table-wrap\">\n<table class=\"content-table\">\n    <thead><tr><th>D50-Bereich<\/th><th>Eigenschaften<\/th><th>Typische Anwendungen<\/th><\/tr><\/thead>\n    <tbody>\n        <tr>\n            <td>Gr\u00f6\u00dferer D50<\/td>\n            <td class=\"wrap\"><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> H\u00f6here Schnittleistung<br><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> H\u00f6here Materialabtragsleistung<br><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Schnellere Verarbeitungsgeschwindigkeit<\/td>\n            <td>Grobschleifen, hocheffizientes L\u00e4ppen, Herstellung von Diamantwerkzeugen<\/td>\n        <\/tr>\n        <tr>\n            <td>Kleiner D50<\/td>\n            <td class=\"wrap\"><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Geringere Oberfl\u00e4chenrauheit<br><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> H\u00f6here Bearbeitungspr\u00e4zision<br><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Bessere Oberfl\u00e4cheng\u00fcte<\/td>\n            <td>Pr\u00e4zisionspolieren, Bearbeitung optischer Komponenten, Halbleiteranwendungen<\/td>\n        <\/tr>\n    <\/tbody>\n<\/table><\/div><\/div><\/div><\/section><section data-block-section class=\"mb-16 lg:mb-32 \" data-block=\"cards\"><div class=\"contain\"><h2 class=\"text-xl lg:text-4xl text-balance mb-6\">D90 &mdash; Grobkornkontrolle<\/h2><div class=\"prose max-w-none\"><p>D90 = 8 &mu;m bedeutet, dass 90 % der Partikel kleiner als 8 &mu;m sind. D90 beschreibt den Grobpartikelanteil, die Kontrolle \u00fcbergro\u00dfer Partikel und die Verteilungsbreite.<\/p><p><strong>Eine gute D90-Kontrolle hilft:<\/strong><\/p><ul style=\"list-style:none;padding:0\"><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Reduzieren Sie das Risiko tiefer Kratzer<\/li><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Verbessern Sie die Verarbeitungskonsistenz<\/li><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Erh\u00f6hen Sie die Produktausbeute<\/li><\/ul><p><strong>Besonders wichtig f\u00fcr:<\/strong> Polieren von Halbleiterwafern, Saphirverarbeitung, Veredelung optischer Komponenten, Pr\u00e4zisionskeramik.<\/p><\/div><\/div><\/section><section data-block-section class=\"mb-16 lg:mb-32 \" data-block=\"cards\"><div class=\"contain\"><h2 class=\"text-xl lg:text-4xl text-balance mb-6\">D100 &mdash; Maximal erfasste Partikelgr\u00f6\u00dfe<\/h2><div class=\"prose max-w-none\"><p>D100 = 12 &mu;m bedeutet, dass die maximal erfasste Partikelgr\u00f6\u00dfe in der Probe etwa 12 &mu;m betr\u00e4gt. D100 dient zur Bewertung der Kontrolle \u00fcbergro\u00dfer Partikel, der Leistungsf\u00e4higkeit des Klassierprozesses und des potenziellen Kratzerrisikos.<\/p><p><strong>Die strenge D100-Steuerung f\u00fcr hochwertiges Pr\u00e4zisionspolieren hilft:<\/strong><\/p><ul style=\"list-style:none;padding:0\"><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Minimieren Sie ungew\u00f6hnliche Kratzer<\/li><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Verbessern Sie die Verarbeitungssicherheit<\/li><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Stellen Sie die Stabilit\u00e4t von Charge zu Charge sicher<\/li><\/ul><\/div><\/div><\/section><section data-block-section class=\"mb-16 lg:mb-32 \" data-block=\"cards\"><div class=\"contain\"><h2 class=\"text-xl lg:text-4xl text-balance mb-6\">Verteilungsbreite<\/h2><div class=\"prose max-w-none\"><p><strong>Spanne = (D90 &minus; D10) \/ D50<\/strong> &mdash; Eine kleinere Spanne bedeutet eine engere Verteilung, eine bessere Klassifizierungsgenauigkeit und eine konsistentere Verarbeitungsleistung.<\/p><div class=\"table-wrap\">\n<table class=\"content-table\">\n    <thead><tr><th>Probe<\/th><th>D10<\/th><th>D50<\/th><th>D90<\/th><th>Spanne<\/th><th>Interpretation<\/th><\/tr><\/thead>\n    <tbody>\n        <tr>\n            <td>Probe A<\/td>\n            <td>2 &mu;m<\/td>\n            <td>5 &mu;m<\/td>\n            <td>8 &mu;m<\/td>\n            <td>1.2<\/td>\n            <td class=\"wrap\"><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Enge Verteilung &mdash; konsistente Bearbeitung<\/td>\n        <\/tr>\n        <tr>\n            <td>Probe B<\/td>\n            <td>1 &mu;m<\/td>\n            <td>5 &mu;m<\/td>\n            <td>15 &mu;m<\/td>\n            <td>2.8<\/td>\n            <td class=\"wrap\"><span style=\"color:#dc2626;font-weight:700\">\u2717<\/span> Breite Verteilung &mdash; geringere Prozesskonstanz<\/td>\n        <\/tr>\n    <\/tbody>\n<\/table><\/div><\/div><\/div><\/section><section data-block-section class=\"mb-16 lg:mb-32 \" data-block=\"cards\"><div class=\"contain\"><h2 class=\"text-xl lg:text-4xl text-balance mb-6\">Beispielbericht<\/h2><div class=\"prose max-w-none\"><div class=\"table-wrap\">\n<table class=\"content-table\">\n    <thead><tr><th>Parameter<\/th><th>Ergebnis<\/th><th>Beschreibung<\/th><\/tr><\/thead>\n    <tbody>\n        <tr><td>D10<\/td><td>2.1 &mu;m<\/td><td>Feinpartikelgehalt<\/td><\/tr>\n        <tr><td>D50<\/td><td>5.0 &mu;m<\/td><td>Hauptarbeitspartikelgr\u00f6\u00dfe<\/td><\/tr>\n        <tr><td>D90<\/td><td>7.8 &mu;m<\/td><td>Kontrollbereich f\u00fcr grobe Partikel<\/td><\/tr>\n        <tr><td>D100<\/td><td>10.5 &mu;m<\/td><td>Maximal erkannte Partikelgr\u00f6\u00dfe<\/td><\/tr>\n    <\/tbody>\n<\/table><\/div><p class=\"mt-6\"><strong>Diese Verteilung zeigt an:<\/strong><\/p><ul style=\"list-style:none;padding:0\"><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Kontrollierter Partikelgr\u00f6\u00dfenbereich<\/li><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Gute Partikelgleichm\u00e4\u00dfigkeit<\/li><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Stabile Schleifleistung<\/li><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Geeignet f\u00fcr Pr\u00e4zisionsschleif- und Polieranwendungen<\/li><\/ul><\/div><\/div><\/section><section data-block-section class=\"mb-16 lg:mb-32 \" data-block=\"cards\"><div class=\"contain\"><h2 class=\"text-xl lg:text-4xl text-balance mb-6\">Einfluss der Partikelgr\u00f6\u00dfe auf die Leistung<\/h2><div class=\"table-wrap\">\n<table class=\"content-table\">\n    <thead><tr><th>Partikelgr\u00f6\u00dfenbereich<\/th><th>Hauptmerkmale<\/th><th>Typische Anwendungen<\/th><\/tr><\/thead>\n    <tbody>\n        <tr><td>Grobe Partikel<\/td><td>Starke Schneidf\u00e4higkeit, hohe Abtragsleistung<\/td><td>Grobschleifen, Schleifwerkzeuge<\/td><\/tr>\n        <tr><td>Mittlere Partikel<\/td><td>Balance zwischen Effizienz und Oberfl\u00e4chenqualit\u00e4t<\/td><td>L\u00e4ppen, Pr\u00e4zisionsbearbeitung<\/td><\/tr>\n        <tr><td>Feine Partikel<\/td><td>Hervorragende Oberfl\u00e4cheng\u00fcte<\/td><td>Pr\u00e4zisionspolieren<\/td><\/tr>\n        <tr><td>Nanopartikel<\/td><td>Ultrafeine Finishing-F\u00e4higkeit<\/td><td>CMP und fortgeschrittenes Polieren<\/td><\/tr>\n    <\/tbody>\n<\/table><\/div><\/div><\/section><section data-block-section class=\"mb-16 lg:mb-32 \" data-block=\"cards\"><div class=\"contain\"><h2 class=\"text-xl lg:text-4xl text-balance mb-6\">G\u00e4ngige Messverfahren<\/h2><div class=\"prose max-w-none\"><p>Drei weit verbreitete Techniken zur Charakterisierung der Partikelgr\u00f6\u00dfe von Diamantpulver.<\/p><div class=\"table-wrap\">\n<table class=\"content-table\">\n    <thead><tr><th>Methode<\/th><th>Funktionen<\/th><\/tr><\/thead>\n    <tbody>\n        <tr>\n            <td>Laserbeugungsanalyse<\/td>\n            <td class=\"wrap\"><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Schnelle Messgeschwindigkeit<br><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Hervorragende Wiederholgenauigkeit<br><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Geeignet f\u00fcr die Qualit\u00e4tskontrolle in der Produktion<\/td>\n        <\/tr>\n        <tr>\n            <td>Dynamische Bildanalyse<\/td>\n            <td class=\"wrap\"><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Misst gleichzeitig Partikelgr\u00f6\u00dfe und Morphologie<br><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Geeignet f\u00fcr die erweiterte Pulverbewertung<\/td>\n        <\/tr>\n        <tr>\n            <td>Rasterelektronenmikroskopie (REM)<\/td>\n            <td class=\"wrap\"><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Direkte Beobachtung der Partikelmorphologie<br><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Geeignet f\u00fcr F&amp;E-Analysen und Qualit\u00e4tsverifizierung<\/td>\n        <\/tr>\n    <\/tbody>\n<\/table><\/div><\/div><\/div><\/section><section data-block-section class=\"mb-16 lg:mb-32 \" data-block=\"cards\"><div class=\"contain\"><h2 class=\"text-xl lg:text-4xl text-balance mb-6\">Qualit\u00e4tsdokumentation von Yuansu Diamond<\/h2><div class=\"prose max-w-none\"><p>Um Kunden bei der vollst\u00e4ndigen Bewertung der Produktleistung zu unterst\u00fctzen, stellt Yuansu Diamond professionelle Qualit\u00e4tsdokumentation bereit.<\/p><div class=\"table-wrap\">\n<table class=\"content-table\">\n    <thead><tr><th>Dokument<\/th><th>Zweck<\/th><\/tr><\/thead>\n    <tbody>\n        <tr><td>Bericht zur Partikelgr\u00f6\u00dfenverteilung (PSD-Bericht)<\/td><td>Daten zur Chargenpartikelgr\u00f6\u00dfe &amp; Verteilung<\/td><\/tr>\n        <tr><td>Technisches Datenblatt (TDS)<\/td><td>Produktspezifikationen &amp; Empfohlene Anwendungen<\/td><\/tr>\n        <tr><td>Sicherheitsdatenblatt (SDS)<\/td><td>Handhabung, Lagerung &amp; Sicherheitsinformationen<\/td><\/tr>\n        <tr><td>Qualit\u00e4tspr\u00fcfbericht<\/td><td>Ergebnisse der Chargenqualit\u00e4tspr\u00fcfung<\/td><\/tr>\n    <\/tbody>\n<\/table><\/div><p class=\"mt-6\"><strong>Qualit\u00e4tspr\u00fcfbericht<\/strong> &mdash; Basierend auf den unterschiedlichen Anwendungsanforderungen kann Yuansu Diamond Folgendes anbieten:<\/p><ul style=\"list-style:none;padding:0\"><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Kundenspezifische Partikelgr\u00f6\u00dfenklassen<\/li><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Ma\u00dfgeschneiderte L\u00f6sungen zur Partikelgr\u00f6\u00dfenverteilung<\/li><li><span style=\"color:#16a34a;font-weight:700\">\u2713<\/span> Anwendungsspezifischer technischer Support<\/li><\/ul><\/div><\/div><\/section><section data-block-section class=\"mb-16 lg:mb-32 last-of-type:mb-0 py-16 lg:py-32 bg-gray-50\" data-block=\"cta\"><div class=\"contain\"><div class=\"prose max-w-none\"><h2 class=\"text-3xl\">Ben\u00f6tigen Sie Hilfe bei der Auswertung eines PSD-Berichts?<\/h2><p>Teilen Sie Ihre Testdaten, Verarbeitungsziele und Anforderungen an die Oberfl\u00e4chenbeschaffenheit mit &mdash; Unser technisches Team kann Ihnen bei der \u00dcberpr\u00fcfung der Partikelgr\u00f6\u00dfenverteilung behilflich sein und eine geeignete Qualit\u00e4t aus dem Yuansu Diamond-Sortiment empfehlen.<\/p><p><a href=\"\/about-us\/contact\/\" class=\"group inline-flex items-center text-sm transition-colors ease-hover gap-3 no-underline rounded-xs bg-secondary px-6 py-3 text-on-secondary hover:bg-secondary-200 hover:text-on-secondary active:bg-secondary-400 active:text-on-secondary focus:text-on-secondary visited:text-on-secondary\">Kontaktieren Sie unser technisches Team<\/a><\/p><\/div><\/div><\/section>","protected":false},"excerpt":{"rendered":"<p>A practical guide to interpreting D10, D50, D90 and D100 values in diamond powder particle size reports, including span calculation and selection by PSD.<\/p>\n","protected":false},"author":1,"featured_media":0,"parent":557,"menu_order":0,"comment_status":"closed","ping_status":"closed","template":"page-sandvik.php","meta":{"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"default","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","ast-disable-related-posts":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"class_list":["post-609","page","type-page","status-publish","hentry"],"_links":{"self":[{"href":"https:\/\/yscltest.aakkkk.com\/de\/wp-json\/wp\/v2\/pages\/609","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/yscltest.aakkkk.com\/de\/wp-json\/wp\/v2\/pages"}],"about":[{"href":"https:\/\/yscltest.aakkkk.com\/de\/wp-json\/wp\/v2\/types\/page"}],"author":[{"embeddable":true,"href":"https:\/\/yscltest.aakkkk.com\/de\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/yscltest.aakkkk.com\/de\/wp-json\/wp\/v2\/comments?post=609"}],"version-history":[{"count":0,"href":"https:\/\/yscltest.aakkkk.com\/de\/wp-json\/wp\/v2\/pages\/609\/revisions"}],"up":[{"embeddable":true,"href":"https:\/\/yscltest.aakkkk.com\/de\/wp-json\/wp\/v2\/pages\/557"}],"wp:attachment":[{"href":"https:\/\/yscltest.aakkkk.com\/de\/wp-json\/wp\/v2\/media?parent=609"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}